Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 % Show Material materials with Aluminium of 0.01 % |
Andere | Rest Cu |
Blei | 0.03 % Show Material materials with Blei of 0.03 % |
Eisen | 0.5 - 1.5 % Show Material materials with Eisen of 0.5 - 1.5 % |
Kohlenstoff | 0.03 % Show Material materials with Kohlenstoff of 0.03 % |
Mangan | 0.6 - 1.2 % Show Material materials with Mangan of 0.6 - 1.2 % |
Nickel | 29 - 31 % Show Material materials with Nickel of 29 - 31 % |
Phosphor | 0.01 % Show Material materials with Phosphor of 0.01 % |
Schwefel | 0.01 % Show Material materials with Schwefel of 0.01 % |
Silizium | 0.3 - 0.7 % Show Material materials with Silizium of 0.3 - 0.7 % |
Zink | 0.5 % Show Material materials with Zink of 0.5 % |