Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 120 - 156 GPa Show Material materials with Elastizitätsmodul of 120 - 156 GPa | Typical for Cast Copper Nickel Grade |
Poissonzahl | 23.0 °C | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | Typical for Cast Copper Nickel Grade |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.8E-5 1/K | Typical for Cast Copper Nickel Grade |
Schmelzpunkt | 1100 - 1240 °C Show Material materials with Schmelzpunkt of 1100 - 1240 °C | Typical for Cast Copper Nickel Grade | |
Spezifische Wärmekapazität | 23.0 °C | 377 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 377 J/(kg·K) | Typical for Cast Copper Nickel Grade |
Wärmeleitfähigkeit | 23.0 °C | 23 - 45 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 23 - 45 W/(m·K) | Typical for Cast Copper Nickel Grade |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 % Show Material materials with Aluminium of 0.01 % |
Andere | Rest Cu, total 0.15 |
Bismut | 0.01 % Show Material materials with Bismut of 0.01 % |
Blei | 0.01 % Show Material materials with Blei of 0.01 % |
Cadmium | 0.02 % Show Material materials with Cadmium of 0.02 % |
Eisen | 0.5 - 1.5 % Show Material materials with Eisen of 0.5 - 1.5 % |
Kohlenstoff | 0.03 % Show Material materials with Kohlenstoff of 0.03 % |
Magnesium | 0.01 % Show Material materials with Magnesium of 0.01 % |
Mangan | 0.6 - 1.2 % Show Material materials with Mangan of 0.6 - 1.2 % |
Nickel | 29 - 31 % Show Material materials with Nickel of 29 - 31 % |
Phosphor | 0.01 % Show Material materials with Phosphor of 0.01 % |
Schwefel | 0.01 % Show Material materials with Schwefel of 0.01 % |
Selen | 0.01 % Show Material materials with Selen of 0.01 % |
Silizium | 0.3 - 0.7 % Show Material materials with Silizium of 0.3 - 0.7 % |
Tellur | 0.01 % Show Material materials with Tellur of 0.01 % |
Zink | 0.5 % Show Material materials with Zink of 0.5 % |