Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 % Show Material materials with Aluminium of 0.01 % |
Andere | total 0.80 |
Blei | 0.3 % Show Material materials with Blei of 0.3 % |
Eisen | 0.2 % Show Material materials with Eisen of 0.2 % |
Kupfer | 85 - 87.5 % Show Material materials with Kupfer of 85 - 87.5 % |
Mangan | 0.2 % Show Material materials with Mangan of 0.2 % |
Nickel | 1.5 - 2.5 % Show Material materials with Nickel of 1.5 - 2.5 % |
Phosphor | 0.05 - 0.4 % Show Material materials with Phosphor of 0.05 - 0.4 % |
Schwefel | 0.05 % Show Material materials with Schwefel of 0.05 % |
Silizium | 0.01 % Show Material materials with Silizium of 0.01 % |
Zink | 0.4 % Show Material materials with Zink of 0.4 % |
Zinn | 11 - 13 % Show Material materials with Zinn of 11 - 13 % |