Chemical properties
Property | Value |
---|---|
Andere | total 0.5 |
Antimon | 0.1 % Show Material materials with Antimon of 0.1 % |
Blei | 0.3 % Show Material materials with Blei of 0.3 % |
Eisen | 0.2 % Show Material materials with Eisen of 0.2 % |
Kupfer | 84 - 87 % Show Material materials with Kupfer of 84 - 87 % |
Nickel | 1.5 - 2.5 % Show Material materials with Nickel of 1.5 - 2.5 % |
Phosphor | 0.2 % Show Material materials with Phosphor of 0.2 % |
Schwefel | 0.05 % Show Material materials with Schwefel of 0.05 % |
Zink | 0.4 % Show Material materials with Zink of 0.4 % |