Chemical properties
Property | Value |
---|---|
Aluminium | 0.02 % Show Material materials with Aluminium of 0.02 % |
Andere | Rest Cu, total 0.8 |
Antimon | 0.5 % Show Material materials with Antimon of 0.5 % |
Arsen | 0.15 % Show Material materials with Arsen of 0.15 % |
Blei | 8.5 - 11 % Show Material materials with Blei of 8.5 - 11 % |
Eisen | 0.2 % Show Material materials with Eisen of 0.2 % |
Mangan | 0.2 % Show Material materials with Mangan of 0.2 % |
Nickel | 0.2 % Show Material materials with Nickel of 0.2 % |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % |
Schwefel | 0.08 % Show Material materials with Schwefel of 0.08 % |
Silizium | 0.02 % Show Material materials with Silizium of 0.02 % |
Zink | 0.8 % Show Material materials with Zink of 0.8 % |
Zinn | 9 - 11 % Show Material materials with Zinn of 9 - 11 % |