Chemical properties
Property | Value |
---|---|
Aluminium | 4.5 - 7 % Show Material materials with Aluminium of 4.5 - 7 % |
Andere | Rest Zn, total 0.5 |
Blei | 0.2 % Show Material materials with Blei of 0.2 % |
Eisen | 2 - 4 % Show Material materials with Eisen of 2 - 4 % |
Kupfer | 64 - 68 % Show Material materials with Kupfer of 64 - 68 % |
Mangan | 1.5 - 4 % Show Material materials with Mangan of 1.5 - 4 % |
Nickel | 3 % Show Material materials with Nickel of 3 % |
Silizium | 0.3 % Show Material materials with Silizium of 0.3 % |
Zinn | 0.3 % Show Material materials with Zinn of 0.3 % |