Chemical properties
Property | Value |
---|---|
Aluminium | 1 - 3 % Show Material materials with Aluminium of 1 - 3 % |
Antimon | 0.05 % Show Material materials with Antimon of 0.05 % |
Blei | 0.3 % Show Material materials with Blei of 0.3 % |
Eisen | 0.5 - 2.5 % Show Material materials with Eisen of 0.5 - 2.5 % |
Kupfer | 55 - 66 % Show Material materials with Kupfer of 55 - 66 % |
Mangan | 1 - 4 % Show Material materials with Mangan of 1 - 4 % |
Nickel | 3 % Show Material materials with Nickel of 3 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |
Zinn | 0.3 % Show Material materials with Zinn of 0.3 % |