Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Material materials with Aluminium of 0.05 % |
Andere | Rest Cu, total 0.5 |
Blei | 0.05 % Show Material materials with Blei of 0.05 % |
Eisen | 0.2 % Show Material materials with Eisen of 0.2 % |
Mangan | 0.7 - 1.3 % Show Material materials with Mangan of 0.7 - 1.3 % |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % |
Silizium | 2.7 - 3.2 % Show Material materials with Silizium of 2.7 - 3.2 % |