Chemical properties
Property | Value |
---|---|
Aluminium | 0.03 % Show Material materials with Aluminium of 0.03 % |
Andere | Rest Cu, total 0.2 |
Blei | 0.01 % Show Material materials with Blei of 0.01 % |
Eisen | 0.03 % Show Material materials with Eisen of 0.03 % |
Mangan | 0.1 - 0.4 % Show Material materials with Mangan of 0.1 - 0.4 % |
Nickel | 0.1 % Show Material materials with Nickel of 0.1 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Silizium | 0.1 - 0.4 % Show Material materials with Silizium of 0.1 - 0.4 % |
Zinn | 0.1 % Show Material materials with Zinn of 0.1 % |