Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 % Show Material materials with Aluminium of 0.01 % |
Andere | Rest Cu, Zn+Cd < 0.05, Alle Total 0.25 |
Bismut | 0.03 % Show Material materials with Bismut of 0.03 % |
Blei | 0.02 % Show Material materials with Blei of 0.02 % |
Cadmium | 0.03 % Show Material materials with Cadmium of 0.03 % |
Nickel | 0.05 - 0.15 % Show Material materials with Nickel of 0.05 - 0.15 % |
Phosphor | 7 - 7.6 % Show Material materials with Phosphor of 7 - 7.6 % |
Silber | 5.5 - 6.5 % Show Material materials with Silber of 5.5 - 6.5 % |
Zink | 0.05 % Show Material materials with Zink of 0.05 % |