Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 % Show Material materials with Aluminium of 0.01 % |
Andere | Rest Cu, Zn+Cd < 0.05, Alle Total 0.25 |
Antimon | 1.8 - 2.2 % Show Material materials with Antimon of 1.8 - 2.2 % |
Bismut | 0.03 % Show Material materials with Bismut of 0.03 % |
Blei | 0.02 % Show Material materials with Blei of 0.02 % |
Cadmium | 0.03 % Show Material materials with Cadmium of 0.03 % |
Phosphor | 5.6 - 6.4 % Show Material materials with Phosphor of 5.6 - 6.4 % |
Zink | 0.05 % Show Material materials with Zink of 0.05 % |