Chemical properties
Property | Value |
---|---|
Aluminium | 1E-3 % Show Material materials with Aluminium of 1E-3 % |
Andere | total 0.30 |
Bismut | 0.03 % Show Material materials with Bismut of 0.03 % |
Blei | 0.03 % Show Material materials with Blei of 0.03 % |
Cadmium | 0.03 % Show Material materials with Cadmium of 0.03 % |
Kupfer | 37 - 39 % Show Material materials with Kupfer of 37 - 39 % |
Mangan | 8.5 - 10.5 % Show Material materials with Mangan of 8.5 - 10.5 % |
Nickel | 5 - 6 % Show Material materials with Nickel of 5 - 6 % |
Phosphor | 8E-3 % Show Material materials with Phosphor of 8E-3 % |
Silber | 26 - 28 % Show Material materials with Silber of 26 - 28 % |
Silizium | 0.05 % Show Material materials with Silizium of 0.05 % |
Zink | 18 - 22 % Show Material materials with Zink of 18 - 22 % |