Chemical properties
Property | Value |
---|---|
Aluminium | 5.5 - 6.5 % Show Material materials with Aluminium of 5.5 - 6.5 % |
Andere | Alle Total 0.5 |
Blei | 0.02 % Show Material materials with Blei of 0.02 % |
Eisen | 1.5 - 2.5 % Show Material materials with Eisen of 1.5 - 2.5 % |
Kupfer | 72 - 78 % Show Material materials with Kupfer of 72 - 78 % |
Mangan | 9 - 14 % Show Material materials with Mangan of 9 - 14 % |
Nickel | 1.5 - 2.5 % Show Material materials with Nickel of 1.5 - 2.5 % |
Silizium | 0.2 % Show Material materials with Silizium of 0.2 % |
Zink | 0.2 % Show Material materials with Zink of 0.2 % |