Chemical properties
Property | Value |
---|---|
Aluminium | 9 - 10 % Show Material materials with Aluminium of 9 - 10 % |
Andere | Rest Cu, total 0.2 |
Blei | 0.02 % Show Material materials with Blei of 0.02 % |
Eisen | 0.5 - 1.5 % Show Material materials with Eisen of 0.5 - 1.5 % |
Mangan | 0.5 % Show Material materials with Mangan of 0.5 % |
Nickel | 1 % Show Material materials with Nickel of 1 % |
Silizium | 0.2 % Show Material materials with Silizium of 0.2 % |
Zink | 0.5 % Show Material materials with Zink of 0.5 % |