Chemical properties
Property | Value |
---|---|
Aluminium | 8.5 - 9.5 % Show Material materials with Aluminium of 8.5 - 9.5 % |
Andere | Rest Cu, total 0.2 |
Blei | 0.02 % Show Material materials with Blei of 0.02 % |
Eisen | 2.5 - 4 % Show Material materials with Eisen of 2.5 - 4 % |
Mangan | 1 - 2 % Show Material materials with Mangan of 1 - 2 % |
Nickel | 3.5 - 5.5 % Show Material materials with Nickel of 3.5 - 5.5 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |
Zink | 0.2 % Show Material materials with Zink of 0.2 % |