Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 % Show Material materials with Aluminium of 0.01 % |
Andere | Rest Zn, total 0.2 |
Blei | 0.02 % Show Material materials with Blei of 0.02 % |
Eisen | 0.25 % Show Material materials with Eisen of 0.25 % |
Kupfer | 46 - 50 % Show Material materials with Kupfer of 46 - 50 % |
Mangan | 0.2 % Show Material materials with Mangan of 0.2 % |
Nickel | 8 - 11 % Show Material materials with Nickel of 8 - 11 % |
Silizium | 0.15 - 0.4 % Show Material materials with Silizium of 0.15 - 0.4 % |
Zinn | 0.2 % Show Material materials with Zinn of 0.2 % |