Chemical properties
Property | Value |
---|---|
Aluminium | 1E-3 % Show Material materials with Aluminium of 1E-3 % |
Andere | total 0.15 |
Bismut | 0.03 % Show Material materials with Bismut of 0.03 % |
Blei | 0.03 % Show Material materials with Blei of 0.03 % |
Cadmium | 13 - 17 % Show Material materials with Cadmium of 13 - 17 % |
Kupfer | 39 - 41 % Show Material materials with Kupfer of 39 - 41 % |
Phosphor | 8E-3 % Show Material materials with Phosphor of 8E-3 % |
Silber | 19 - 21 % Show Material materials with Silber of 19 - 21 % |
Silizium | 0.05 % Show Material materials with Silizium of 0.05 % |
Zink | 23 - 27 % Show Material materials with Zink of 23 - 27 % |