Chemical properties
Property | Value |
---|---|
Aluminium | 1E-3 % Show Material materials with Aluminium of 1E-3 % |
Andere | total 0.15 |
Bismut | 0.03 % Show Material materials with Bismut of 0.03 % |
Blei | 0.03 % Show Material materials with Blei of 0.03 % |
Cadmium | 14.5 - 18.5 % Show Material materials with Cadmium of 14.5 - 18.5 % |
Kupfer | 34.5 - 36.5 % Show Material materials with Kupfer of 34.5 - 36.5 % |
Phosphor | 8E-3 % Show Material materials with Phosphor of 8E-3 % |
Silber | 20 - 22 % Show Material materials with Silber of 20 - 22 % |
Silizium | 0.3 - 0.7 % Show Material materials with Silizium of 0.3 - 0.7 % |
Zink | 24.5 - 28.5 % Show Material materials with Zink of 24.5 - 28.5 % |