Chemical properties
Property | Value |
---|---|
Aluminium | 1E-3 % Show Material materials with Aluminium of 1E-3 % |
Andere | total 0.15 |
Bismut | 0.03 % Show Material materials with Bismut of 0.03 % |
Blei | 0.03 % Show Material materials with Blei of 0.03 % |
Cadmium | 15.5 - 19.5 % Show Material materials with Cadmium of 15.5 - 19.5 % |
Kupfer | 29 - 31 % Show Material materials with Kupfer of 29 - 31 % |
Phosphor | 8E-3 % Show Material materials with Phosphor of 8E-3 % |
Silber | 24 - 26 % Show Material materials with Silber of 24 - 26 % |
Silizium | 0.05 % Show Material materials with Silizium of 0.05 % |
Zink | 25.5 - 29.5 % Show Material materials with Zink of 25.5 - 29.5 % |