Chemical properties
Property | Value |
---|---|
Aluminium | 1E-3 % Show Material materials with Aluminium of 1E-3 % |
Andere | total 0.15 |
Bismut | 0.03 % Show Material materials with Bismut of 0.03 % |
Blei | 0.03 % Show Material materials with Blei of 0.03 % |
Cadmium | 0.03 % Show Material materials with Cadmium of 0.03 % |
Kupfer | 54 - 56 % Show Material materials with Kupfer of 54 - 56 % |
Phosphor | 8E-3 % Show Material materials with Phosphor of 8E-3 % |
Silber | 4 - 6 % Show Material materials with Silber of 4 - 6 % |
Silizium | 0.05 - 0.25 % Show Material materials with Silizium of 0.05 - 0.25 % |
Zink | 38 - 42 % Show Material materials with Zink of 38 - 42 % |