Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Material materials with Aluminium of 0.05 % |
Andere | Rest Cu, each 0.05, total 0.3 |
Antimon | 0.02 % Show Material materials with Antimon of 0.02 % |
Arsen | 0.02 % Show Material materials with Arsen of 0.02 % |
Bismut | 5E-3 % Show Material materials with Bismut of 5E-3 % |
Blei | 0.05 % Show Material materials with Blei of 0.05 % |
Eisen | 0.2 % Show Material materials with Eisen of 0.2 % |
Kohlenstoff | 0.05 % Show Material materials with Kohlenstoff of 0.05 % |
Magnesium | 0.05 % Show Material materials with Magnesium of 0.05 % |
Mangan | 29 - 31 % Show Material materials with Mangan of 29 - 31 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Selen | 5E-3 % Show Material materials with Selen of 5E-3 % |
Silizium | 0.05 % Show Material materials with Silizium of 0.05 % |
Tellur | 5E-3 % Show Material materials with Tellur of 5E-3 % |
Zink | 0.2 % Show Material materials with Zink of 0.2 % |
Zinn | 0.05 % Show Material materials with Zinn of 0.05 % |