Chemical properties
Property | Value |
---|---|
Aluminium | 0.1 % Show Material materials with Aluminium of 0.1 % |
Andere | Rest Cu, each 0.1, total 0.5 |
Blei | 0.2 % Show Material materials with Blei of 0.2 % |
Eisen | 0.7 % Show Material materials with Eisen of 0.7 % |
Mangan | 0.2 % Show Material materials with Mangan of 0.2 % |
Silizium | 28 - 32 % Show Material materials with Silizium of 28 - 32 % |
Zink | 0.2 % Show Material materials with Zink of 0.2 % |
Zinn | 0.2 % Show Material materials with Zinn of 0.2 % |