Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Material materials with Aluminium of 0.05 % |
Andere | Rest Cu, each 0.1, total 0.5 |
Bismut | 5E-3 % Show Material materials with Bismut of 5E-3 % |
Blei | 0.05 % Show Material materials with Blei of 0.05 % |
Eisen | 0.1 % Show Material materials with Eisen of 0.1 % |
Niobium | 2 % Show Material materials with Niobium of 2 % |
Phosphor | 0.1 % Show Material materials with Phosphor of 0.1 % |
Silizium | 0.05 % Show Material materials with Silizium of 0.05 % |
Tellur | 5E-3 % Show Material materials with Tellur of 5E-3 % |
Zinn | 0.2 % Show Material materials with Zinn of 0.2 % |
Zirkonium | 49 - 53 % Show Material materials with Zirkonium of 49 - 53 % |