Chemical properties
Property | Value |
---|---|
Andere | total 0.03. excluded Ag, P |
Antimon | 4E-4 % Show Material materials with Antimon of 4E-4 % |
Arsen | 5E-4 % Show Material materials with Arsen of 5E-4 % |
Bismut | 2E-4 % Show Material materials with Bismut of 2E-4 % |
Blei | 5E-4 % Show Material materials with Blei of 5E-4 % |
Cadmium | 1E-4 % Show Material materials with Cadmium of 1E-4 % |
Eisen | 1E-3 % Show Material materials with Eisen of 1E-3 % |
Kupfer | 99.99 % Show Material materials with Kupfer of 99.99 % |
Mangan | 5E-4 % Show Material materials with Mangan of 5E-4 % |
Nickel | 1E-3 % Show Material materials with Nickel of 1E-3 % |
Phosphor | 3E-4 - 6E-3 % Show Material materials with Phosphor of 3E-4 - 6E-3 % |
Schwefel | 1.5E-3 % Show Material materials with Schwefel of 1.5E-3 % |
Silber | 2.5E-3 % Show Material materials with Silber of 2.5E-3 % |
Tellur | 2E-4 % Show Material materials with Tellur of 2E-4 % |
Zink | 1E-4 % Show Material materials with Zink of 1E-4 % |
Zinn | 2E-4 % Show Material materials with Zinn of 2E-4 % |