Chemical properties
Property | Value |
---|---|
Aluminium | 2E-3 % Show Material materials with Aluminium of 2E-3 % |
Andere | Cu: including Ag to max. 0.015% and O to 0.06%, each 0.002 |
Bismut | 5E-4 % Show Material materials with Bismut of 5E-4 % |
Blei | 5E-3 % Show Material materials with Blei of 5E-3 % |
Eisen | 2E-3 % Show Material materials with Eisen of 2E-3 % |
Kupfer | 99.9 % Show Material materials with Kupfer of 99.9 % |
Nickel | 2E-3 % Show Material materials with Nickel of 2E-3 % |
Phosphor | 1E-3 % Show Material materials with Phosphor of 1E-3 % |
Zink | 2E-3 % Show Material materials with Zink of 2E-3 % |
Zinn | 2E-3 % Show Material materials with Zinn of 2E-3 % |