Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Material materials with Aluminium of 0.05 % |
Andere | Cu: including Ag to max. 0.015% and O to 0.06%, each 0.002 |
Arsen | 5E-3 % Show Material materials with Arsen of 5E-3 % |
Blei | 0.1 % Show Material materials with Blei of 0.1 % |
Eisen | 0.05 % Show Material materials with Eisen of 0.05 % |
Kupfer | 99.5 % Show Material materials with Kupfer of 99.5 % |
Nickel | 0.02 % Show Material materials with Nickel of 0.02 % |
Phosphor | 0.06 % Show Material materials with Phosphor of 0.06 % |
Zink | 0.05 % Show Material materials with Zink of 0.05 % |