Chemical properties
Property | Value |
---|---|
Aluminium | 0.2 % Show Material materials with Aluminium of 0.2 % |
Andere | Cu: including Ag to max. 0.015% and O to 0.06% |
Blei | 1.5 % Show Material materials with Blei of 1.5 % |
Eisen | 0.5 % Show Material materials with Eisen of 0.5 % |
Kupfer | 96 % Show Material materials with Kupfer of 96 % |
Nickel | 0.2 % Show Material materials with Nickel of 0.2 % |
Zink | 1.5 % Show Material materials with Zink of 1.5 % |
Zinn | 0.5 % Show Material materials with Zinn of 0.5 % |