Chemical properties
Property | Value |
---|---|
Andere | Rest Cu, total 0.2 |
Blei | 0.02 % Show Material materials with Blei of 0.02 % |
Eisen | 1.5 - 2.5 % Show Material materials with Eisen of 1.5 - 2.5 % |
Kobalt | 0.1 % Show Material materials with Kobalt of 0.1 % |
Kohlenstoff | 0.05 % Show Material materials with Kohlenstoff of 0.05 % |
Mangan | 1.5 - 2.5 % Show Material materials with Mangan of 1.5 - 2.5 % |
Nickel | 29 - 32 % Show Material materials with Nickel of 29 - 32 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.05 % Show Material materials with Schwefel of 0.05 % |
Zink | 0.5 % Show Material materials with Zink of 0.5 % |
Zinn | 0.5 % Show Material materials with Zinn of 0.5 % |