Chemical properties
Property | Value |
---|---|
Aluminium | 0.4 % Show Material materials with Aluminium of 0.4 % |
Andere | Rest Zn, total 0.4, Al+Fe+Ni+Sn+Others total< 1.7%, in case of CuZn38Pb4 (CW609N) Pb < 4.2% |
Blei | 3.5 % Show Material materials with Blei of 3.5 % |
Eisen | 0.6 % Show Material materials with Eisen of 0.6 % |
Kupfer | 57 % Show Material materials with Kupfer of 57 % |
Nickel | 0.5 % Show Material materials with Nickel of 0.5 % |
Zinn | 0.6 % Show Material materials with Zinn of 0.6 % |