Chemical properties
Property | Value |
---|---|
Aluminium | 8.5 - 10.5 % Show Material materials with Aluminium of 8.5 - 10.5 % |
Andere | Rest Cu, total 1.0 |
Blei | 0.02 % Show Material materials with Blei of 0.02 % |
Eisen | 4 - 5 % Show Material materials with Eisen of 4 - 5 % |
Kohlenstoff | 0.1 % Show Material materials with Kohlenstoff of 0.1 % |
Mangan | 0.8 - 2.5 % Show Material materials with Mangan of 0.8 - 2.5 % |
Nickel | 4 - 5 % Show Material materials with Nickel of 4 - 5 % |
Silizium | 0.15 % Show Material materials with Silizium of 0.15 % |