Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 % Show Material materials with Aluminium of 0.01 % |
Andere | Rest Cu, total 1.0 |
Antimon | 0.2 % Show Material materials with Antimon of 0.2 % |
Arsen | 0.1 % Show Material materials with Arsen of 0.1 % |
Bismut | 5E-3 % Show Material materials with Bismut of 5E-3 % |
Blei | 27 - 33 % Show Material materials with Blei of 27 - 33 % |
Eisen | 0.5 % Show Material materials with Eisen of 0.5 % |
Mangan | 0.3 % Show Material materials with Mangan of 0.3 % |
Phosphor | 0.08 % Show Material materials with Phosphor of 0.08 % |
Silizium | 0.02 % Show Material materials with Silizium of 0.02 % |
Zinn | 1 % Show Material materials with Zinn of 1 % |