Chemical properties
Property | Value |
---|---|
Aluminium | 0.02 % Show Material materials with Aluminium of 0.02 % |
Andere | Rest Cu, total 1.0 |
Antimon | 0.3 % Show Material materials with Antimon of 0.3 % |
Blei | 4 - 6 % Show Material materials with Blei of 4 - 6 % |
Eisen | 0.3 % Show Material materials with Eisen of 0.3 % |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % |
Zink | 1 % Show Material materials with Zink of 1 % |
Zinn | 9 - 11 % Show Material materials with Zinn of 9 - 11 % |