Chemical properties
Property | Value |
---|---|
Aluminium | 0.2 - 0.25 % Show Material materials with Aluminium of 0.2 - 0.25 % |
Andere | Rest Zn |
Antimon | 0.05 % Show Material materials with Antimon of 0.05 % |
Arsen | 0.05 % Show Material materials with Arsen of 0.05 % |
Blei | 0.15 - 0.2 % Show Material materials with Blei of 0.15 - 0.2 % |
Eisen | 0.15 - 0.2 % Show Material materials with Eisen of 0.15 - 0.2 % |
Kupfer | 59 - 61 % Show Material materials with Kupfer of 59 - 61 % |
Mangan | 0.15 - 0.2 % Show Material materials with Mangan of 0.15 - 0.2 % |
Nickel | 0.2 % Show Material materials with Nickel of 0.2 % |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % |
Silizium | 0.7 - 1.1 % Show Material materials with Silizium of 0.7 - 1.1 % |
Zinn | 0.2 - 0.25 % Show Material materials with Zinn of 0.2 - 0.25 % |