Abmessung
Property | Value |
---|---|
Dimensions | Dicke |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 42 % Show Material materials with Dehnung of 42 % |
Härte, Vickers | 20.0 °C | 40 - 65 [-] Show Material materials with Härte, Vickers of 40 - 65 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 100 MPa Show Material materials with Streckgrenze Rp 0,2 of 100 MPa |
Zugfestigkeit | 20.0 °C | 200 - 250 MPa Show Material materials with Zugfestigkeit of 200 - 250 MPa |