Abmessung
Property | Value |
---|---|
Dimensions | Durchmesser |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 5 % Show Material materials with Dehnung of 5 % |
Elongation A100 | 20.0 °C | 3 % Show Material materials with Elongation A100 of 3 % |
Härte, Brinell | 20.0 °C | 100 [-] Show Material materials with Härte, Brinell of 100 [-] |
Härte, Vickers | 20.0 °C | 110 [-] Show Material materials with Härte, Vickers of 110 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 330 MPa Show Material materials with Streckgrenze Rp 0,2 of 330 MPa |
Zugfestigkeit | 20.0 °C | 350 MPa Show Material materials with Zugfestigkeit of 350 MPa |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 5.86E+7 S/m Show Material materials with Elektrische Leitfähigkeit of 5.86E+7 S/m |
spezifischer Widerstand | 20.0 °C | 1.71E-8 Ω·m Show Material materials with spezifischer Widerstand of 1.71E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Andere | total 0.0065 |
Antimon | 4E-4 % Show Material materials with Antimon of 4E-4 % |
Arsen | 5E-4 % Show Material materials with Arsen of 5E-4 % |
Bismut | 2E-4 % Show Material materials with Bismut of 2E-4 % |
Blei | 5E-4 % Show Material materials with Blei of 5E-4 % |
Eisen | 1E-3 % Show Material materials with Eisen of 1E-3 % |
Schwefel | 1.5E-3 % Show Material materials with Schwefel of 1.5E-3 % |
Silber | 2.5E-3 % Show Material materials with Silber of 2.5E-3 % |
Tellur | 2E-4 % Show Material materials with Tellur of 2E-4 % |