Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 8.9 g/cm³ Show Material materials with Dichte of 8.9 g/cm³ | Typical for Wrought Copper Pure / Low Alloyed Copper |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 30 % Show Material materials with Dehnung of 30 % | |
Elastizitätsmodul | 23.0 °C | 126.5 GPa Show Material materials with Elastizitätsmodul of 126.5 GPa | |
Poissonzahl | 23.0 °C | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | Typical for Wrought Copper Pure / Low Alloyed Copper |
Schubmodule | 23.0 °C | 48 GPa Show Material materials with Schubmodule of 48 GPa | Typical for Wrought Copper Pure / Low Alloyed Copper |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20.0 °C | 1.7E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.7E-5 1/K | |
100.0 °C | 1.7E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.7E-5 1/K | ||
Schmelzpunkt | 1082 °C Show Material materials with Schmelzpunkt of 1082 °C | ||
Spezifische Wärmekapazität | 23.0 °C | 377 - 420 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 377 - 420 J/(kg·K) | Typical for Wrought Copper Pure / Low Alloyed Copper |
Wärmeleitfähigkeit | 23.0 °C | 380 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 380 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 5.40E+7 - 5.70E+7 S/m Show Material materials with Elektrische Leitfähigkeit of 5.40E+7 - 5.70E+7 S/m |
spezifischer Widerstand | 23.0 °C | 1.75E-8 - 1.85E-8 Ω·m Show Material materials with spezifischer Widerstand of 1.75E-8 - 1.85E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Andere | total 0.0065. excluded Ag, O |
Bismut | 5E-4 % Show Material materials with Bismut of 5E-4 % |
Phosphor | 1E-3 - 7E-3 % Show Material materials with Phosphor of 1E-3 - 7E-3 % |
Silber | 0.08 - 0.12 % Show Material materials with Silber of 0.08 - 0.12 % |