Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.3 g/cm³ Show Material materials with Dichte of 8.3 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 20 % Show Material materials with Dehnung of 20 % | |
Elastizitätsmodul | 23.0 °C | 110 - 130 GPa Show Material materials with Elastizitätsmodul of 110 - 130 GPa | Typical for Wrought Copper High Copper Alloy |
Elongation A100 | 23.0 °C | 12 % Show Material materials with Elongation A100 of 12 % | |
Härte, Brinell | 23.0 °C | 120 [-] Show Material materials with Härte, Brinell of 120 [-] | |
Härte, Vickers | 23.0 °C | 120 [-] Show Material materials with Härte, Vickers of 120 [-] | |
Streckgrenze Rp 0,2 | 23.0 °C | 190 MPa Show Material materials with Streckgrenze Rp 0,2 of 190 MPa | |
Zugfestigkeit | 23.0 °C | 410 MPa Show Material materials with Zugfestigkeit of 410 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 - 1.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 - 1.8E-5 1/K | Typical for Wrought Copper High Copper Alloy |
Schmelzpunkt | 855 - 1090 °C Show Material materials with Schmelzpunkt of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy | |
Spezifische Wärmekapazität | 23.0 °C | 360 - 420 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |
Chemical properties