Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 6.3 g/cm³ Show Material materials with Dichte of 6.3 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Bending Fatigue Strength | 23.0 °C | 100 MPa Show Material materials with Bending Fatigue Strength of 100 MPa | |
Dehnung A50 | 20.0 °C | 8 % Show Material materials with Dehnung A50 of 8 % | |
23.0 °C | 8 % Show Material materials with Dehnung A50 of 8 % | ||
Elastizitätsmodul | 20.0 °C | 86 GPa Show Material materials with Elastizitätsmodul of 86 GPa | |
Härte, Brinell | 20.0 °C | 100 [-] Show Material materials with Härte, Brinell of 100 [-] | |
23.0 °C | 100 [-] Show Material materials with Härte, Brinell of 100 [-] | ||
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Zinc Aluminium |
Streckgrenze Rp 0,2 | 20.0 °C | 220 MPa Show Material materials with Streckgrenze Rp 0,2 of 220 MPa | |
23.0 °C | 220 MPa Show Material materials with Streckgrenze Rp 0,2 of 220 MPa | ||
Zugfestigkeit | 20.0 °C | 937 MPa Show Material materials with Zugfestigkeit of 937 MPa | |
23.0 °C | 370 MPa Show Material materials with Zugfestigkeit of 370 MPa | ||
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.2E-5 - 2.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.2E-5 - 2.8E-5 1/K | Typical for Zinc Aluminium |
Schmelzpunkt | 375 - 485 °C Show Material materials with Schmelzpunkt of 375 - 485 °C | Typical for Zinc Aluminium | |
Spezifische Wärmekapazität | 23.0 °C | 393 - 525 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 393 - 525 J/(kg·K) | Typical for Zinc Aluminium |
Wärmeleitfähigkeit | 20.0 °C | 115 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 115 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 1.62E+7 S/m Show Material materials with Elektrische Leitfähigkeit of 1.62E+7 S/m |
spezifischer Widerstand | 20.0 °C | 6.2E-8 Ω·m Show Material materials with spezifischer Widerstand of 6.2E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Aluminium | 8 - 8.8 % Show Material materials with Aluminium of 8 - 8.8 % |
Andere | Rest Zn |
Blei | 6E-3 % Show Material materials with Blei of 6E-3 % |
Cadmium | 6E-3 % Show Material materials with Cadmium of 6E-3 % |
Eisen | 0.06 % Show Material materials with Eisen of 0.06 % |
Kupfer | 0.8 - 1.3 % Show Material materials with Kupfer of 0.8 - 1.3 % |
Magnesium | 0.02 - 0.03 % Show Material materials with Magnesium of 0.02 - 0.03 % |
Nickel | 0.02 % Show Material materials with Nickel of 0.02 % |
Silizium | 0.05 % Show Material materials with Silizium of 0.05 % |
Zink | 89.73 % Show Material materials with Zink of 89.73 % |
Zinn | 3E-3 % Show Material materials with Zinn of 3E-3 % |