Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 5 g/cm³ Show Material materials with Dichte of 5 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Bending Fatigue Strength | 23.0 °C | 145 MPa Show Material materials with Bending Fatigue Strength of 145 MPa | |
Dehnung A50 | 20.0 °C | 2.5 % Show Material materials with Dehnung A50 of 2.5 % | |
23.0 °C | 2.5 % Show Material materials with Dehnung A50 of 2.5 % | ||
Elastizitätsmodul | 20.0 °C | 78 GPa Show Material materials with Elastizitätsmodul of 78 GPa | |
Härte, Brinell | 20.0 °C | 120 [-] Show Material materials with Härte, Brinell of 120 [-] | |
23.0 °C | 120 [-] Show Material materials with Härte, Brinell of 120 [-] | ||
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Zinc Aluminium |
Streckgrenze Rp 0,2 | 20.0 °C | 370 MPa Show Material materials with Streckgrenze Rp 0,2 of 370 MPa | |
23.0 °C | 370 MPa Show Material materials with Streckgrenze Rp 0,2 of 370 MPa | ||
Zugfestigkeit | 20.0 °C | 425 MPa Show Material materials with Zugfestigkeit of 425 MPa | |
23.0 °C | 425 MPa Show Material materials with Zugfestigkeit of 425 MPa | ||
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.2E-5 - 2.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.2E-5 - 2.8E-5 1/K | Typical for Zinc Aluminium |
Schmelzpunkt | 375 - 485 °C Show Material materials with Schmelzpunkt of 375 - 485 °C | Typical for Zinc Aluminium | |
Spezifische Wärmekapazität | 23.0 °C | 393 - 525 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 393 - 525 J/(kg·K) | Typical for Zinc Aluminium |
Wärmeleitfähigkeit | 20.0 °C | 126 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 126 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 1.74E+7 S/m Show Material materials with Elektrische Leitfähigkeit of 1.74E+7 S/m |
spezifischer Widerstand | 20.0 °C | 5.8E-8 Ω·m Show Material materials with spezifischer Widerstand of 5.8E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Aluminium | 25 - 28 % Show Material materials with Aluminium of 25 - 28 % |
Andere | Rest Zn |
Blei | 6E-3 % Show Material materials with Blei of 6E-3 % |
Cadmium | 6E-3 % Show Material materials with Cadmium of 6E-3 % |
Eisen | 0.1 % Show Material materials with Eisen of 0.1 % |
Kupfer | 2 - 2.5 % Show Material materials with Kupfer of 2 - 2.5 % |
Magnesium | 0.01 - 0.02 % Show Material materials with Magnesium of 0.01 - 0.02 % |
Nickel | 0.02 % Show Material materials with Nickel of 0.02 % |
Silizium | 0.08 % Show Material materials with Silizium of 0.08 % |
Zink | 69.27 % Show Material materials with Zink of 69.27 % |
Zinn | 3E-3 % Show Material materials with Zinn of 3E-3 % |