Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.8 g/cm³ Show Material materials with Dichte of 8.8 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Durchmesser |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 50 % Show Material materials with Dehnung of 50 % |
Elongation A100 | 20.0 °C | 40 % Show Material materials with Elongation A100 of 40 % |
Härte, Vickers | 20.0 °C | 85 - 115 [-] Show Material materials with Härte, Vickers of 85 - 115 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 150 MPa Show Material materials with Streckgrenze Rp 0,2 of 150 MPa |
Zugfestigkeit | 20.0 °C | 260 - 380 MPa Show Material materials with Zugfestigkeit of 260 - 380 MPa |
Chemical properties
Property | Value |
---|---|
Andere | Rest Cu, total 0.5 |
Blei | 0.05 % Show Material materials with Blei of 0.05 % |
Eisen | 0.8 % Show Material materials with Eisen of 0.8 % |
Mangan | 0.7 % Show Material materials with Mangan of 0.7 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Silizium | 0.8 - 2 % Show Material materials with Silizium of 0.8 - 2 % |
Zink | 1.5 % Show Material materials with Zink of 1.5 % |