Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.8 g/cm³ Show Material materials with Dichte of 8.8 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Durchmesser |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 50 % Show Material materials with Dehnung of 50 % |
Elastizitätsmodul | 20.0 °C | 105 GPa Show Material materials with Elastizitätsmodul of 105 GPa |
Elongation A100 | 20.0 °C | 40 % Show Material materials with Elongation A100 of 40 % |
Härte, Brinell | 20.0 °C | 85 - 115 [-] Show Material materials with Härte, Brinell of 85 - 115 [-] |
Härte, Vickers | 20.0 °C | 90 - 120 [-] Show Material materials with Härte, Vickers of 90 - 120 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 260 MPa Show Material materials with Streckgrenze Rp 0,2 of 260 MPa |
Zugfestigkeit | 20.0 °C | 380 MPa Show Material materials with Zugfestigkeit of 380 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 20.0 °C | 1.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.8E-5 1/K |
100.0 °C | 1.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.8E-5 1/K | |
Schmelzpunkt | 970 - 1025 °C Show Material materials with Schmelzpunkt of 970 - 1025 °C | |
Wärmeleitfähigkeit | 20.0 °C | 38 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 38 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 3.80E+6 - 4.00E+6 S/m Show Material materials with Elektrische Leitfähigkeit of 3.80E+6 - 4.00E+6 S/m |
spezifischer Widerstand | 20.0 °C | 2.5E-7 - 2.63E-7 Ω·m Show Material materials with spezifischer Widerstand of 2.5E-7 - 2.63E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Material materials with Aluminium of 0.05 % |
Andere | Rest Cu, total 0.5 |
Blei | 0.05 % Show Material materials with Blei of 0.05 % |
Eisen | 0.2 % Show Material materials with Eisen of 0.2 % |
Mangan | 0.7 - 1.3 % Show Material materials with Mangan of 0.7 - 1.3 % |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % |
Silizium | 2.7 - 3.2 % Show Material materials with Silizium of 2.7 - 3.2 % |
Zink | 0.4 % Show Material materials with Zink of 0.4 % |