Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.2 g/cm³ Show Material materials with Dichte of 8.2 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Dicke |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 45 % Show Material materials with Dehnung A50 of 45 % |
Härte, Vickers | 20.0 °C | 80 [-] Show Material materials with Härte, Vickers of 80 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 170 MPa Show Material materials with Streckgrenze Rp 0,2 of 170 MPa |
Zugfestigkeit | 20.0 °C | 400 MPa Show Material materials with Zugfestigkeit of 400 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 4 - 6 % Show Material materials with Aluminium of 4 - 6 % |
Andere | Rest Cu, total 0.5 |
Eisen | 0.15 % Show Material materials with Eisen of 0.15 % |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % |
Zink | 4 - 6 % Show Material materials with Zink of 4 - 6 % |
Zinn | 0.3 - 1.5 % Show Material materials with Zinn of 0.3 - 1.5 % |