Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.9 g/cm³ Show Material materials with Dichte of 8.9 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Dicke |
Mechanisch
Property | Temperature | Value |
---|---|---|
Härte, Vickers | 20.0 °C | 70 - 100 [-] Show Material materials with Härte, Vickers of 70 - 100 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 100 MPa Show Material materials with Streckgrenze Rp 0,2 of 100 MPa |
Zugfestigkeit | 20.0 °C | 290 MPa Show Material materials with Zugfestigkeit of 290 MPa |
Chemical properties
Property | Value |
---|---|
Andere | Rest Cu, total 0.1 |
Blei | 0.02 % Show Material materials with Blei of 0.02 % |
Eisen | 0.3 % Show Material materials with Eisen of 0.3 % |
Kobalt | 0.1 % Show Material materials with Kobalt of 0.1 % |
Kohlenstoff | 0.05 % Show Material materials with Kohlenstoff of 0.05 % |
Mangan | 0.5 % Show Material materials with Mangan of 0.5 % |
Nickel | 24 - 26 % Show Material materials with Nickel of 24 - 26 % |
Schwefel | 0.05 % Show Material materials with Schwefel of 0.05 % |
Zink | 0.5 % Show Material materials with Zink of 0.5 % |
Zinn | 0.03 % Show Material materials with Zinn of 0.03 % |