Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.9 g/cm³ Show Material materials with Dichte of 8.9 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Wanddicke |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 30 % Show Material materials with Dehnung of 30 % |
Härte, Vickers | 20.0 °C | 90 - 125 [-] Show Material materials with Härte, Vickers of 90 - 125 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 150 MPa Show Material materials with Streckgrenze Rp 0,2 of 150 MPa |
Zugfestigkeit | 20.0 °C | 420 MPa Show Material materials with Zugfestigkeit of 420 MPa |
Chemical properties
Property | Value |
---|---|
Andere | Rest Cu, total 0.2 |
Blei | 0.02 % Show Material materials with Blei of 0.02 % |
Eisen | 1.5 - 2.5 % Show Material materials with Eisen of 1.5 - 2.5 % |
Kobalt | 0.1 % Show Material materials with Kobalt of 0.1 % |
Kohlenstoff | 0.05 % Show Material materials with Kohlenstoff of 0.05 % |
Mangan | 1.5 - 2.5 % Show Material materials with Mangan of 1.5 - 2.5 % |
Nickel | 29 - 32 % Show Material materials with Nickel of 29 - 32 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.05 % Show Material materials with Schwefel of 0.05 % |
Zink | 0.5 % Show Material materials with Zink of 0.5 % |
Zinn | 0.5 % Show Material materials with Zinn of 0.5 % |