Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.9 g/cm³ Show Material materials with Dichte of 8.9 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Dicke |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 35 % Show Material materials with Dehnung of 35 % |
Härte, Vickers | 20.0 °C | 80 - 120 [-] Show Material materials with Härte, Vickers of 80 - 120 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 120 MPa Show Material materials with Streckgrenze Rp 0,2 of 120 MPa |
Zugfestigkeit | 20.0 °C | 350 - 420 MPa Show Material materials with Zugfestigkeit of 350 - 420 MPa |
Chemical properties
Property | Value |
---|---|
Andere | Rest Cu, total 0.2 |
Blei | 0.2 % Show Material materials with Blei of 0.2 % |
Eisen | 0.4 - 1 % Show Material materials with Eisen of 0.4 - 1 % |
Kobalt | 0.1 % Show Material materials with Kobalt of 0.1 % |
Kohlenstoff | 0.05 % Show Material materials with Kohlenstoff of 0.05 % |
Mangan | 0.5 - 1.5 % Show Material materials with Mangan of 0.5 - 1.5 % |
Nickel | 30 - 32 % Show Material materials with Nickel of 30 - 32 % |
Phosphor | 0.2 % Show Material materials with Phosphor of 0.2 % |
Schwefel | 0.05 % Show Material materials with Schwefel of 0.05 % |
Zink | 0.5 % Show Material materials with Zink of 0.5 % |
Zinn | 0.05 % Show Material materials with Zinn of 0.05 % |