Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.6 g/cm³ Show Material materials with Dichte of 8.6 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Dicke,Durchmesser |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 40 - 45 % Show Material materials with Dehnung of 40 - 45 % |
Dehnung A50 | 20.0 °C | 35 % Show Material materials with Dehnung A50 of 35 % |
Härte, Vickers | 20.0 °C | 80 - 130 [-] Show Material materials with Härte, Vickers of 80 - 130 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 160 - 230 MPa Show Material materials with Streckgrenze Rp 0,2 of 160 - 230 MPa |
Zugfestigkeit | 20.0 °C | 360 - 480 MPa Show Material materials with Zugfestigkeit of 360 - 480 MPa |
Chemical properties
Property | Value |
---|---|
Andere | Rest Zn, total 0.2 |
Blei | 0.05 % Show Material materials with Blei of 0.05 % |
Eisen | 0.3 % Show Material materials with Eisen of 0.3 % |
Kupfer | 61 - 64 % Show Material materials with Kupfer of 61 - 64 % |
Mangan | 0.5 % Show Material materials with Mangan of 0.5 % |
Nickel | 9 - 11 % Show Material materials with Nickel of 9 - 11 % |