Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 2.84 g/cm³ Show Material materials with Dichte of 2.84 g/cm³ |
Thermisch
Property | Value |
---|---|
Schmelzpunkt | 543 - 643 °C Show Material materials with Schmelzpunkt of 543 - 643 °C |
Chemical properties
Property | Value |
---|---|
Eisen | 0.3 % Show Material materials with Eisen of 0.3 % |
Kupfer | 6.8 % Show Material materials with Kupfer of 6.8 % |
Magnesium | 0.02 % Show Material materials with Magnesium of 0.02 % |
Mangan | 0.4 % Show Material materials with Mangan of 0.4 % |
Silizium | 0.2 % Show Material materials with Silizium of 0.2 % |
Titan | 0.2 % Show Material materials with Titan of 0.2 % |
Vanadium | 0.15 % Show Material materials with Vanadium of 0.15 % |
Zink | 0.1 % Show Material materials with Zink of 0.1 % |
Zirkonium | 0.25 % Show Material materials with Zirkonium of 0.25 % |