Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.7 g/cm³ Show Material materials with Dichte of 8.7 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Dicke |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 15 % Show Material materials with Dehnung A50 of 15 % |
Härte, Vickers | 20.0 °C | 110 - 140 [-] Show Material materials with Härte, Vickers of 110 - 140 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 260 MPa Show Material materials with Streckgrenze Rp 0,2 of 260 MPa |
Zugfestigkeit | 20.0 °C | 380 - 470 MPa Show Material materials with Zugfestigkeit of 380 - 470 MPa |
Chemical properties
Property | Value |
---|---|
Andere | Rest Zn, total 0.2 |
Blei | 0.5 - 1.5 % Show Material materials with Blei of 0.5 - 1.5 % |
Eisen | 0.3 % Show Material materials with Eisen of 0.3 % |
Kupfer | 60 - 63 % Show Material materials with Kupfer of 60 - 63 % |
Mangan | 0.5 % Show Material materials with Mangan of 0.5 % |
Nickel | 11 - 13 % Show Material materials with Nickel of 11 - 13 % |