Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.4 g/cm³ Show Material materials with Dichte of 8.4 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Durchmesser |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 5 % Show Material materials with Dehnung of 5 % |
Härte, Brinell | 20.0 °C | 170 [-] Show Material materials with Härte, Brinell of 170 [-] |
Härte, Vickers | 20.0 °C | 180 [-] Show Material materials with Härte, Vickers of 180 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 450 MPa Show Material materials with Streckgrenze Rp 0,2 of 450 MPa |
Zugfestigkeit | 20.0 °C | 650 MPa Show Material materials with Zugfestigkeit of 650 MPa |
Chemical properties
Property | Value |
---|---|
Andere | Rest Zn, total 0.2 |
Blei | 1 - 2.5 % Show Material materials with Blei of 1 - 2.5 % |
Eisen | 0.3 % Show Material materials with Eisen of 0.3 % |
Kupfer | 42 - 45 % Show Material materials with Kupfer of 42 - 45 % |
Mangan | 4.5 - 6 % Show Material materials with Mangan of 4.5 - 6 % |
Nickel | 11 - 13 % Show Material materials with Nickel of 11 - 13 % |
Zinn | 0.2 % Show Material materials with Zinn of 0.2 % |