Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.7 g/cm³ Show Material materials with Dichte of 8.7 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 20 % Show Material materials with Dehnung of 20 % | |
Elastizitätsmodul | 23.0 °C | 120 - 140 GPa Show Material materials with Elastizitätsmodul of 120 - 140 GPa | Typical for Wrought Copper Nickel Silver Grade |
Elongation A100 | 23.0 °C | 12 % Show Material materials with Elongation A100 of 12 % | |
Härte, Brinell | 23.0 °C | 130 [-] Show Material materials with Härte, Brinell of 130 [-] | |
Härte, Vickers | 23.0 °C | 130 [-] Show Material materials with Härte, Vickers of 130 [-] | |
Poissonzahl | 23.0 °C | 0.32 [-] Show Material materials with Poissonzahl of 0.32 [-] | Typical for Wrought Copper Nickel Silver Grade |
Streckgrenze Rp 0,2 | 23.0 °C | 280 MPa Show Material materials with Streckgrenze Rp 0,2 of 280 MPa | |
Zugfestigkeit | 23.0 °C | 420 MPa Show Material materials with Zugfestigkeit of 420 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 - 1.9E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 - 1.9E-5 1/K | Typical for Wrought Copper Nickel Silver Grade |
Schmelzpunkt | 875 - 1135 °C Show Material materials with Schmelzpunkt of 875 - 1135 °C | Typical for Wrought Copper Nickel Silver Grade | |
Spezifische Wärmekapazität | 23.0 °C | 377 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 377 J/(kg·K) | Typical for Wrought Copper Nickel Silver Grade |
Wärmeleitfähigkeit | 23.0 °C | 21 - 116 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 21 - 116 W/(m·K) | Typical for Wrought Copper Nickel Silver Grade |
Chemical properties
Property | Value |
---|---|
Andere | Rest Zn, total 0.2 |
Blei | 0.1 - 1.5 % Show Material materials with Blei of 0.1 - 1.5 % |
Eisen | 0.3 % Show Material materials with Eisen of 0.3 % |
Kupfer | 59.5 - 62.5 % Show Material materials with Kupfer of 59.5 - 62.5 % |
Mangan | 0.7 % Show Material materials with Mangan of 0.7 % |
Nickel | 17 - 19 % Show Material materials with Nickel of 17 - 19 % |
Zinn | 0.2 % Show Material materials with Zinn of 0.2 % |